310 Refractory Anchors frameworks and are produced for a wide range of solid, fired fiber and block refractory anchors affirming that the precise evaluation of material, measurements, dividing designs and welding strategies are chosen for a mooring framework which is extremely fundamental for holding the hard-headed material and guarantees the covering execution.
Refractory anchors have the following features- Great tensile strength, Excellent stability at high temperatures, Reliable performance, Precise designing, Durability, Sturdy construction, Hardness.
Chemical Composition of Stainless Steel 310 Anchors
Grade 310 |
Fe |
Cr |
Ni |
Mn |
Si |
C |
P |
S |
min. |
48.3 |
24.0 |
19.0 |
- |
- |
- |
- |
- |
max. |
57.0 |
26.0 |
22.0 |
2.0 |
1.5 |
0.08 |
0.045 |
0.03 |
Mechanical Properties of Stainless Steel 310 Anchors
Grade |
Tensile Strength (MPa) min |
Yield Strength 0.2% Proof (MPa) min |
Elongation (% in 50mm) min |
Hardness |
Rockwell B (HR B) max |
Brinell (HB) max |
310 |
620 |
310 |
30 |
90 |
198 |
310H also has a requirement for a grain size of ASTM No 7 or coarser. |
Physical Properties of Stainless Steel 310 Anchors
Density (kg/m3) |
Elastic Modulus (GPa) |
Mean Coefficient of Thermal Expansion (m/m/0C) |
Thermal Conductivity (W/m.K) |
Specific Heat 0-1000C (J/kg.K) |
Electrical Resistivity (n.m) |
0-1000C |
0-3150C |
0-5380C |
at 1000C |
at 5000C |
8.0 |
200 |
16 |
- |
500 |
16 |
16 |
500 |
25 |
Grade Specification for Stainless Steel 310 Anchors
Grade |
UNS No |
Old British |
Euronorm |
Swedish SS |
Japanese JIS |
BS |
En |
No |
Name |
310 |
S31008 |
- |
- |
- |
X10CrNi18-8 |
- |
- |
These comparisons are approximate only. The list is intended as a comparison of functionally similar materials not as a schedule of contractual equivalents. If exact equivalents are needed original specifications must be consulted. |